Struktur butir cacat 99,999% Al;
Reagen Barker, Cahya Polarisasi
Al-1% Si as-cast spesimen karo partikel Si ing matriks α-Al;"Si Biru" etch
Al-7,12% Si, as-cast, kanthi dendrit α-Al primer lan eutektik a-Al/Si;"Si Biru" etch
Al -11,7% Si, as-cast, kanthi dendrit a-Al primer lan eutektik α-Al/Si;"Si Biru" etch
Al -12% Si, as-cast, cedhak eutektik, "Si Biru" etch
AI -12% Si, as-cast, cedhak eutektik;Reagen Weck, Cahya Polarisasi
Na-Modified Al - 12% Si, as-cast, cedhak eutektik, "Si Biru" etch
Na-Modified Al -12% Si, as-cast, near eutektik Weck's Reagent, Polarized Light
Al - 12,9% Si, gravitasi die cast, "Si Biru" etch
Al- 12,9% Si-0,04% Sr, gravitasi die cast, "Si Biru" etch
Al-19,85% Si, as-cast, hipereutetik, Si primer plus eutektik, Reagen Weck - sel eutektik, 200X
Al-25% Si, as-cast, hypereutectic, Si primer lan eutektik α-Al/Si, Reagen Weck
Al - 50% Si, minangka-cast, retak Si utami lan eutektik, "Si Biru" etch
Kembar ing polikristalin 99.9999% Si, banyu as-cast 75% NaOH, Nomarski DIC
diagram fase AI - SIi