MP35N minangka alloy nikel lan kobalt kromium molibdenum non-magnetik.Kekuwatan tensile dhuwur, nganti 300ksi [2068MPa]) ketangguhan ductility apik lan resistance karat Resistance banget kanggo vulkanisasi, oksidasi suhu dhuwur lan kinerja embrittlement hidrogen .Kinerja unik liwat hardening karya, transformasi phase lan perawatan tuwa.Yen digunakake ing kondisi hardening, suhu operasi -200~315°C, lan suhu maksimum sing disaranake 750 derajat Fahrenheit (399 derajat c)
C | Mn | P | S | Si | Cr | Ni | Mo | Co | Ti | B | Te |
≦ 0.03 | ≦ 0.15 | ≦ 0,015 | ≦ 0,010 | ≦ 0.15 | 19.0 21.0 | 33.0 37.0 | 9.0 10.50 | ≧ 35.0 | ≦ 1.0 | ≦ 0.01 | ≦ 1.0 |
Kapadhetan (g/cm3) | Titik lebur (°C) | Koefisien ekspansi (m/(m·°C)(21-93°C)) |
8.43 | 1440 | 12.8×10E-6 |
kahanan | σb MPa | σ0.2 MPa | φ % | Ψ % | Kekerasan HRC |
Solusi padhet + Kerja kadhemen | 1758 | 1551 | 12 | 50 | 45 |
Solusi padhet + Kerja kadhemen +Sepuh | 1792 | 1585 | 8 | 35 | 38 min |
AMS5758, AMS5844, AMS5845, ANSI/ASTM F562, NACE MR0175
•Resistance apik kanggo Vulkanisasi, oksidasi suhu dhuwur, garing, kabut uyah lan asam mineral sing paling akeh.
•Resistance apik kanggo retak korosi stres ing lingkungan sing atos lan kekuatan dhuwur.
•Resistance dhuwur kanggo karat lokal, kayata korosi pitting lan korosi crevice.
MP35N alloy bisa digunakake kanggo perawatan medical, banyu segara, lenga lan gas Wells, kimia lan fastener, spring,
Komponen magnetik lan bagean peralatan lingkungan pangolahan panganan